Feb 09, 2026 Lăsaţi un mesaj

inconel 600 Grosimea plăcii

 

Grosimea plăcii de oțel Inconel 600, grosimea plăcii de metal din aliaj de 600 (mm), grosimea plăcii de oțel din aliaj de nichel 600, grosimea plăcii de oțel UNS N06600 (mm).

 

Uns N06600 Tabel cu grosimea foii

Ecartament (ga) Grosimea oțelului (in.) Grosimea oțelului (mm) Grosimea aluminiului (in.) Grosimea aluminiului (mm)
3 0.2391 6.07 0.2294 5.83
4 0.2242 5.69 0.2043 5.19
5 0.2092 5.31 0.1819 4.62
6 0.1943 4.94 0.162 4.11
7 0.1793 4.55 0.1443 3.67
8 0.1644 4.18 0.1285 3.26
9 0.1495 3.80 0.1144 2.91
10 0.1345 3.42 0.1019 2.59
11 0.1196 3.04 0.0907 2.30
12 0.1046 2.66 0.0808 2.05
13 0.0897 2.28 0.072 1.83
14 0.0747 1.90 0.0641 1.63
15 0.0673 1.71 0.0571 1.45
16 0.0598 1.52 0.0508 1.29
17 0.0538 1.37 0.0453 1.15
18 0.0478 1.21 0.0403 1.02
19 0.0418 1.06 0.0359 0.91
20 0.0359 0.91 0.032 0.81
21 0.0329 0.84 0.0285 0.72
22 0.0299 0.76 0.0253 0.64
23 0.0269 0.68 0.0226 0.57
24 0.0239 0.61 0.0201 0.51
25 0.0209 0.53 0.0179 0.45
26 0.0179 0.45 0.0159 0.40
27 0.0164 0.42 0.0142 0.36
28 0.0149 0.38 0.0126 0.32
29 0.0135 0.34 0.0113 0.29
30 0.012 0.30 0.01 0.25
31 0.0105 0.27 0.0089 0.23
32 0.0097 0.25 0.008 0.20
33 0.009 0.23 0.0071 0.18
34 0.0082 0.21 0.0063 0.16
35 0.0075 0.19 0.0056 0.14
36 0.0067 0.17

 

Tabel cu grosimea plăcilor din aliaj 600

Ecartament LB/mp. Ft. LB/Sq In. Toleranța ecartamentului plăcii
72 inchi lățime 96 inchi lățime
3/16 0.1875 8.579 0.05958 +.045″ -.010″ +.050″ -.010″
7/32 0.2187 9.870 0.06854
1/4 0.2500 11.162 0.07750
5/16 0.3125 13.746 0.09546
3/8 0.3750 16.496 0.11456 +.055″ -.010″ +.060″ -.010″
7/16 0.4375 19.080 0.13250
1/2 0.5000 21.633 0.15044
9/16 0.5625 24.247 0.16838
5/8 0.6250 26.831 0.18633
11/16 0.6875 29.415 0.20427
3/4 0.7500 32.123 0.22308 +.060″ -.010″ +.065″ -.010″
13/16 0.8125 34.707 0.24102
7/8 0.8750 37.291 0.25897
15/16 0.9375 39.875 0.27691
1 1.0000 42.665 0.29628 +.070″ -.010″ +.075 -.010″
1-1/8 1.1250 47.833 0.33217
1-1/4 1.2500 53.001 0.36806
1-3/8 1.3750 58.169 0.40395
1-1/2 1.5000 63.337 0.43984
1-3/4 1.7500 73.672 0.51161
2 2.0000 84.008 0.58339 +.125″ -.010″ +.150″ -.010″
2-1/8 2.1250 89.610 0.62229
2-1/4 2.2500 94.777 0.65817
2-1/2 2.5000 105.113 0.72995
2-3/4 2.7500 115.449 0.80173
3 3.0000 126.301 0.87709 +.150″ -.010″ +.160″ -.010″
3-1/2 3.5000 146.972 1.02064
4 4.0000 168.264 1.16850 +.180″ -.010″ +.200″ -.010

 

Tabel cu grosimea bobinei de nichel 600

grosime (mm) 1000 Mai mică sau egală cu Lățimea < 1250 (mm) 630 Mai mică sau egală cu Lățimea < 1000 (mm) 1250 Mai mică sau egală cu Lățimea < 1550 (mm)
0,40 Mai mic sau egal cu T < 0,60 ±0.035 ±0.035 -
1,25 Mai mic sau egal cu T < 1,60 ±0.060 ±0.055 ±0.060
1,60 Mai mic sau egal cu T < 2,00 ±0.070 ±0.065 ±0.080
0,25 Mai mic sau egal cu T < 0,40 ±0.035 ±0.030 -
0,80 Mai mic sau egal cu T < 1,00 ±0.050 ±0.040 ±0.050
0,60 Mai mic sau egal cu T < 0,80 ±0.040 ±0.040 -
1,00 Mai mic sau egal cu T < 1,25 ±0.055 ±0.050 ±0.060

 

modular-1

ss@gneesteel.com

Vizualizați dimensiunile plăcii de oțel Inconel 600 (mm), dimensiunile plăcilor standard și dimensiunile bobinei, tabelul cu dimensiunile bobinei și dimensiunile plăcilor din oțel inoxidabil Gnee Steel.

Trimite anchetă

whatsapp

Telefon

E-mail

Anchetă