Dimensiuni Standard Inconel 601 Bara rotunda
| Diametrul sau Lăţime (mm) |
Greutate pe metru | Zona Secțională | Perimetru | |||
| Pătrat (kg) |
Rundă (kg) |
Pătrat (cm²) |
Rundă (cm²) |
Pătrat (cm) |
Rundă (cm) |
|
| 5.0 | 0.20 | 0.15 | 0.25 | 0.20 | 2.0 | 1.57 |
| 5.5 | 0.24 | 0.19 | 0.30 | 0.24 | 2.2 | 1.78 |
| 6.0 | 0.28 | 0.22 | 0.36 | 0.28 | 2.4 | 1.88 |
| 7.0 | 0.38 | 0.30 | 0.49 | 0.38 | 2.8 | 2.20 |
| 8.0 | 0.50 | 0.39 | 0.64 | 0.50 | 3.2 | 2.51 |
| 9.0 | 0.64 | 0.50 | 0.81 | 0.64 | 3.6 | 2.83 |
| 10 | 0.73 | 0.63 | 1.00 | 0.79 | 4.0 | 3.14 |
| 11 | 0.95 | 0.75 | 1.21 | 0.95 | 4.4 | 3.46 |
| 12 | 1.13 | 0.89 | 1.44 | 1.13 | 4.8 | 3.77 |
| 14 | 1.54 | 1.21 | 1.96 | 1.54 | 5.6 | 4.40 |
| 16 | 2.01 | 1.58 | 2.56 | 2.01 | 6.4 | 5.03 |
| 18 | 2.54 | 2.00 | 3.24 | 2.54 | 7.2 | 5.65 |
| 20 | 3.14 | 2.47 | 4.00 | 3.14 | 8.0 | 6.28 |
| 22 | 3.80 | 2.98 | 4.84 | 3.80 | 8.8 | 6.91 |
| 25 | 4.91 | 3.85 | 6.25 | 4.91 | 10.0 | 7.85 |
| 28 | 6.15 | 4.83 | 7.84 | 6.16 | 11.2 | 8.80 |
| 32 | 8.04 | 6.31 | 10.24 | 8.04 | 12.8 | 10.05 |
| 36 | 10.17 | 7.99 | 12.96 | 10.18 | 14.4 | 11.31 |
| 40 | 12.56 | 9.86 | 16.00 | 12.57 | 16.0 | 12.57 |
| 45 | 15.90 | 12.49 | 20.25 | 15.90 | 18.0 | 14.14 |
| 50 | 19.62 | 15.41 | 25.00 | 19.64 | 20.0 | 15.71 |
| 56 | 24.62 | 19.34 | 31.36 | 24.63 | 22.4 | 17.59 |
| 63 | 31.16 | 24.47 | 36.69 | 31.17 | 25.2 | 19.79 |
| 71 | 39.57 | 31.08 | 50.41 | 39.59 | 28.4 | 22.31 |
| 80 | 50.24 | 39.46 | 64.00 | 50.27 | 32.0 | 25.13 |
Inconel UNS N06601 Toleranță bară rotundă strălucitoare
| Inconel 601 Toleranță bară rotundă Seria ISO „H” în MM | ||||||||
|---|---|---|---|---|---|---|---|---|
| Dimensiune (mm) | H12 | H11 | H10 | H9 | H8 | H7 | H6 | H5 |
| Peste 180 - 250 | +0.46/0 | +0.29/0 | +0.185/0 | +0.115/0 | +0.072/0 | +0.046/0 | +0.029/0 | +0.02/0 |
| Peste 120 - 180 | +0.4/0 | +0.25/0 | +0.16/0 | +0.1/0 | +0.063/0 | +0.04/0 | +0.025/0 | +0.018/0 |
| Peste 80 - 120 | +0.35/0 | +0.22/0 | +0.14/0 | +0.087/0 | +0.054/0 | +0.035/0 | +0.022/0 | +0.015/0 |
| Peste 50 - 80 | +0.3/0 | +0.19/0 | +0.12/0 | +0.074/0 | +0.046/0 | +0.03/0 | +0.019/0 | +0.013/0 |
| Peste 30 - 50 | +0.25/0 | +0.16/0 | +0.1/0 | +0.062/0 | +0.039/0 | +0.025/0 | +0.016/0 | +0.011/0 |
| Peste 18 - 30 | +0.21/0 | +0.13/0 | +0.084/0 | +0.052/0 | +0.033/0 | +0.021/0 | +0.013/0 | +0.009/0 |
| Peste 10 - 18 | +0.18/0 | +0.11/0 | +0.07/0 | +0.043/0 | +0.027/0 | +0.018/0 | +0.011/0 | +0.008/0 |
| Peste 6 - 10 | +0.15/0 | +0.09/0 | +0.058/0 | +0.036/0 | +0.022/0 | +0.015/0 | +0.009/0 | +0.006/0 |
| Peste 3 - 6 | +0.12/0 | +0.075/0 | +0.048/0 | +0.03/0 | +0.018/0 | +0.012/0 | +0.008/0 | +0.005/0 |
| ~ la 3 | +0.1/0 | +0.06/0 | +0.04/0 | +0.025/0 | +0.014/0 | +0.01/0 | +0.006/0 | +0.004/0 |