Hastelloy C-2000 Raw Materials Alloy Sheet
Density:8.9 g/cm3, Melting Point:1325-1370 ºC
1,Hastelloy C22(N06022)Tensile strength of nickel-based alloys Rm N/mm2:690
2,Hastelloy C22(N06022)Yield strength of nickel base alloy RP0.2N/mm2:283
3,Hastelloy C22(N06022)Elongation of nickel base alloy A5 %:40
1)Hastelloy C22 alloys are suitable for a variety of chemical process industries containing oxidizing and reducing media.
2) The high content of molybdenum and chromium makes the alloy resistant to chloride ions, and tungsten further improves its corrosion resistance.
3)Hastelloy C22 is one of the only materials capable of resisting the corrosion of moist chlorine, hypochlorite and chlorine dioxide solutions.
4)The alloy has excellent corrosion resistance to high concentrations of salt chloride solutions (such as ferric chloride and copper chloride).