Feb 02, 2026 Lăsaţi un mesaj

Dimensiuni fitinguri Incoloy 800/800H/800HT

Tabel de dimensiuni fitinguri de țeavă 800 (mm), tabel de dimensiuni de fitinguri de țeavă din aliaj 800/800H/800HT PDF, diagramă de dimensiuni standard de fitinguri de țeavă Incoloy 800.

 

Dimensiuni 800/800H/800HT armături pentru țevi de sudare cap la cap din aliaj

ASME b16.9 Fitinguri
Dimensiunea normală a conductei
Fiting pentru țevi ANSI b16 9 O
D Y
Perete Grosime T
(Sch. cot țeavă)
Coturi LR 45 de gradeCentru către FaţăB Coturi SR 45 de grade
Greutate
Coturi LR 90 de gradeCentru către FaţăA Coturi LR 90 de grade Greutate In Dedesubt Coturi SR 90 de gradeCentru către FaţăA Coturi SR 90 de grade Greutate In Dedesubt
milimetru inch. milimetru milimetru Programa milimetru kilogram milimetru kilogram milimetru kilogram
15 1/2" 21.3 2.78 STD 15.9 0.04 38.1 0.08
      3.73 X.S 15.9 0.05 38.1 0.10
20 3/4" 26.7 2.87 STD 11.1 0.04 28.6 0.08
      3.91 X.S 11.1 0.05 28.6 0.11
25 1" 33.4 3.38 STD 22.2 0.09 38.1 0.15 25.4 0.11
      4.55 X.S 22.2 0.11 38.1 0.19 25.4 0.14
32 11/4" 42.2 3.56 STD 25.4 0.14 47.6 0.28 31.75 0.18
      4.85 X.S 25.4 0.2 47.6 0.39 31.75 0.24
40 11/2" 48.3 3.68 STD 28.6 0.2 57.1 0.4 38.1 0.26
      5.08 X.S 28.6 0.25 57.1 0.5 38.1 0.35
50 2" 60.3 3.91 STD 34.9 0.36 76.2 0.72 50.8 0.5
      5.54 X.S 34.9 0.5 76.2 1.0 50.8 0.68
65 21/2" 73.0 5.16 STD 44.4 0.73 95.2 1.46 63.5 0.95
      7.01 X.S 44.4 0.91 95.2 1.82 63.5 1.27
80 3" 88.9 5.49 STD 50.8 1.1 114.3 2.18 76.2 1.45
      7.62 X.S 50.8 1.45 114.3 2.86 76.2 1.95
100 4" 114.3 6.02 STD 63.5 2.1 152.4 4.2 101.6 2.8
      8.56 X.S 63.5 2.9 152.4 5.7 101.6 3.9
125 5" 141.3 6.65 STD 79.4 3.4 190.0 6.8 127.0 4.8
      9.5 X.S 79.4 5.0 190.0 10.0 127.0 6.5
150 6" 168.3 7.11 STD 95.2 5.1 229.0 10.1 152.4 6.8
      10.97 X.S 95.2 7.7 229.0 15.3 152.4 10.2
200 8" 219.1 8.18 STD 127.0 10.2 305.0 20.4 203.0 13.6
      12.7 X.S 127.0 15.5 305.0 30.9 203.0 20.9
250 10" 273.9 9.27 STD 159.0 18.1 381.0 36.1 254.0 24.1
      12.7 X.S 159.0 24.4 381.0 48.8 254.0 32.5
300 12" 323.9 9.52 STD 190.0 26.6 457.0 53.1 305.0 35.4
      12.7 X.S 190.0 35.0 457.0 70.0 305.0 46.7
350 14" 355.6 9.52 STD 222.0 34.1 533.0 68.1 356.0 45.4
      12.7 X.S 222.0 45.0 533.0 90.0 356.0 60.0
400 16" 406.4 9.52 STD 254.0 45.0 610.0 89.3 406.0 59.5
      12.7 X.S 254.0 59.0 610.0 118.0 406.0 78.7
450 18" 457.0 9.52 STD 286.0 56.5 686.0 113.0 457.0 75.6
      12.7 X.S 286.0 75.0 686.0 150.0 457.0 100.0
500 20" 508.0 9.52 STD 318.0 85.0 762.0 140.0 508.0 93.5
      12.7 X.S 318.0 112.5 762.0 186.0 508.0 124.0
600 24" 610.00 9.52 STD 381.0 101.5 914.0 203.0 610.0 135.0
      12.7 X.S 381.0 134.5 914.0 269.0 610.0 179.0

Trimite anchetă

whatsapp

Telefon

E-mail

Anchetă