În calitate de furnizor și producător de top în China, GNEE Steel oferă produse din aliaje pe bază de nichel-eficiente din punct de vedere al costurilor.
- Trimiteți e-mail:ss@gneesteel.com
- Tel:+8615824687445
flanges are excellent at forming and welding. While Alloy X is primarily known for its heat and oxidation resistance, these flanges also have good resistance to chloride stress corrosion cracking. Its corrosion resistance to SCC means these ASTM B564 UNS N06002 flanges are a very valuable asset in the petrochemical industry, where alloys need to combine high mechanical strength and corrosion resistance.
| ASTM B564 / ASME SB564 | |
| 1/2" NB TO 64" NB | |
| Class 150#, Class 300#, Class 400#, Class 600#, Class 900#, Class 1500#, Class 2500# or As Per Custom Requirement PN 6, PN 10, PN 16, PN 25 and PN 40 etc |
|
| Sch 10s TO Sch XXS or As Per Custom Requirement | |
| C | P | S | ||||||||
| 8.00 – 10.00 | 20.50 – 23.00 | 17.00 – 20.00 | 1.00 max | 0.05 – 0.15 | 0.50 – 2.50 | 1.00 max | 0.04 max | 0.03 max |
| Yield Strength (0.2%Offset) | ||||
| 8.22 g/cm | 1355 degree | 655 MPa | 240 MPa | 35 |

Tag-uri populare: , aliaj pentru convertoare catalitice, aliaj pentru finisare, aliaj pentru măcinare, aliaj pentru temperare, HASTELLOY MATERIAL PIPING Aliaj, conducte din oțel inoxidabil fără sudură
O pereche de
Tub din aliaj Hastelloy WUrmătoarea
Țevi fără sudură din aliaj Hastelloy WS-ar putea sa-ti placa si
Trimite anchetă